Directions: On a dry and clean surface work the liming wax into the grain with Liberon Ultrafine Steel Wool (0000) or a lint-free cloth and remove excess. Allow 3 minutes to dry. Remove white haze using a cloth and Neutral Black Bison Paste Wax, or for a water-resistant finish use Liberon Finishing Oil. Apply a second coat of wax or a further coat of oil and then wax if required. The more coats of oil the greater the water resistance. Buff to a soft finish.
Directions: On a dry and clean surface work the liming wax into the grain with Liberon Ultrafine Steel Wool (0000) or a lint-free cloth and remove excess. Allow 3 minutes to dry. Remove white haze using a cloth and Neutral Black Bison Paste Wax, or for a water-resistant finish use Liberon Finishing Oil. Apply a second coat of wax or a further coat of oil and then wax if required. The more coats of oil the greater the water resistance. Buff to a soft finish.